Title: Fabrication of Hybrid Surface Composite of Aluminium Alloy using Friction Stir Processing Technique
Authors: Patel, Kevin
Keywords: Mechanical 2020
Project Report
Project Report 2020
Mechanical Project Report
20MME
20MMCC
20MMCC07
Friction Stir Processing
Multi-pass
Al2O3
Surface Composite
AA5083
AA6061
B4C
CNT
Tool Tilt Angle
CAD/CAM 2020
CAD/CAM
CAD/CAM
CAD/CAM 2020
Issue Date: 1-Jun-2022
Publisher: Institute of Technology
Series/Report no.: 20MMCC07;
Abstract: Friction Stir Processing (FSP) is a new process for producing aluminium alloy surface composites. Most composite fabrication processes modify the bulk of the material, whereas FSP simply changes the workpiece's surface properties while keeping the below-surface qualities the same as the parent material. The aluminium alloy AA5083 is noted for its outstanding performance in harsh environments. AA6061 is known for its good weldability and resistance towards corrosion. Due to their good mechanical properties they are used in heavy duty structures like truck frames, ships, Aerospace vehicles, Boilers, Motorboats and Rivets. Surface composite made using two kinds of reinforcement are known as hybrid surface composite, Al2O3 and B4C were used as ceramic particles while MWCNT were used as lubricant particles. AA6061-Al2O3/CNT hybrid surface composite showed 17.5% lower wear rate and 8% lower COF value than AA6061-B4C/CNT hybrid surface composite. Hybrid Surface Composites prepared using FSP increased hardness of base material up to 99 HV. Tool tilt angle from 1 to 3 degree was used on AA6061-Al2O3/CNT Hybrid Surface composite which were then tested for mechanical properties and wear characteristics. Results showed that hybrid surface composite produced using 1 degree of tool tilt angle and 2 passes of FSP showed higher hardness value of 78 HV but because of low material flow during the process lubricant phase particles were not distributed evenly and caused higher wear of 236 micron. Comparing all the results, composite produced by using 2 degree and 2 pass of FSP showed better overall results of 75 HV of hardness, lower rate of wear (153 micron) and 0.3577 value of COF.
URI: http://10.1.7.192:80/jspui/handle/123456789/11294
Appears in Collections:Dissertation, ME (CAD/CAM)

Files in This Item:
File Description SizeFormat 
20MMCC07.pdf20MMCC0725.59 MBAdobe PDFThumbnail
View/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.